| 1895 - 1104 стор.
...horizontally in the liquid near the top of the solution by a silver rod riveted through its center. To prevent the disintegrated silver which is formed on the anode from falling1 upon the kathode, the anode shall be wrapped around with pure filter paper, secured at the... | |
| National Academy of Sciences (U.S.) - 1888 - 840 стор.
...horizontally in the liquid near the top of the solution by a silver rod riveted through its center. To prevent the disintegrated silver which is formed on the anode from falling upon the kathode, the anode shall be wrapped around with pure filter paper, secured at the back by... | |
| Great Britain - 1894 - 610 стор.
...millimetres in thickness. This is supported horizontally in the liquid near the top of the solution by a platinum wire passed through holes in the plate at...formed on the anode from falling on to the kathode, the auode should be wrapped round with pure filter paper, secured at the buck with sealing wax. The liquid... | |
| 1891 - 680 стор.
...in the liquid near the top of the solution by a platinum 'A ire (tossed through holes in the plates at opposite corners. To prevent the disintegrated...which is formed on the anode from falling on to the cathode, the anode should be wrapped round with pure filter paper, secured at the back with a little... | |
| British Association for the Advancement of Science - 1892 - 1258 стор.
...millimetres in thickness. This is supported horizontally in the liquid near the top of the solution by a platinum wire passed through holes in the plate at...round with pure filter paper, secured at the back with sealing wax. The liquid should consist of a neutral solution of pure silver nitrate, containing about... | |
| British Association for the Advancement of Science - 1892 - 1146 стор.
...millimetres in thickness. This is supported horizontally in the liquid near the top of the solution by a platinum wire passed through holes in the plate at...falling on to the kathode, the anode should be wrapped round1 with pure filter paper, secured at the back with sealing wax. The liquid should consist of a... | |
| 1892 - 608 стор.
...3 mm. in thickness. "This is supported horizontally in the liquid near the top of the solution by a platinum wire passed through holes in the plate at...opposite corners. To prevent the disintegrated silver from the anode from falling on the kathode, the anode should be wrapped around with pure filter paper... | |
| 1893 - 630 стор.
...millimetres in thickness. Thia is supported horizontally in the liquid near the top of the solution by a platinum wire passed through holes in the plate at...which is formed on the anode from falling on to the cathode, the anode should be wrapped round with pure filter paper, secured at the back with sealing-wax.... | |
| American Institute of Electrical Engineers - 1893 - 780 стор.
...millimetres in thickness. This is supported horizontally in the liquid near the top of the solution, by a platinum wire passed through holes in the plate at...disintegrated silver which is formed on the anode from falling onto the cathode, the anode should be wrapped around with pure filter paper, secured at the back with... | |
| 1893
...millimetres in thickness. This is supported horizontally in the liquid near the top of the solution, by a platinum wire passed through holes in the plate at...disintegrated silver which is formed on the anode from falling onto the cathode, the anode should be wrapped around with pure filter paper, secured at the back with... | |
| |